This work investigates defect formation in an advanced 300 mm bipolar silicon p-technology for analog applications. The study focuses on the relationship between the initial substrate state, the sequence of buried-layer implantations, and the cumulative thermal budget imposed by subsequent process steps. The type of implantation (p or n) used for the formation of bipolar process blocks (PNP or NPN) condition the type of defects. The influence of first PNP process block based on high dose p-type implantation on defects formation is investigated. We highlight for the first time the use of innovative industrial complementary failure-analysis-related characterization tools, including Light Scattering Tomography (LST), Pattern Wafer Geometry Metrology (PWG) and Micro-Photoluminescence (PL) imaging to monitor defects formation during the flow. Insufficiently prepared substrates being more prone to defect generation during the bipolar flow, we have identified the close relationship of process steps (implantation, annealing and epitaxy collector), combined with sensitivity of p-substrates, towards metallic contamination. An internal gettering consisting of an optimized oxidizing treatment is finally developed to significantly improve defect management (dislocations and crystalline defects) and mitigate metallic contamination trapping, leading to a more robust and reliable bipolar integration.
Topic
semiconductor marketheterojunction bipolar transistorsdefects dislocationsprocess development
Author
A. Abbadie, J. Le Corre, B. Gominski, Y. Ouzaid, G. Avenier, A. Martiz, V. Samu